TC FABRIC COTTON AND POLYESTER BASE FABRIC FOR ARTIFICIAL LEATHER
1. Structure & Weaving Parameters
TC (Tetoron/Cotton) woven base fabric is the most classic and widely used traditional substrate in the synthetic leather industry. Made by blending polyester (Tetoron, T) with cotton (C), it delivers a balanced combination of strength, dimensional stability, moisture management, and cost-effectiveness. It is the dominant backing fabric for shoe linings, bags, and mid-to-entry-level garment leather.
Core principle: polyester provides strength, abrasion resistance, and dimensional stability; cotton contributes softness, moisture absorption, and dye affinity. The blending ratio determines whether the hand feel is crisp (high polyester) or soft (high cotton).
| Parameter | Typical Range / Description |
| Material Composition | Polyester (T) + Cotton (C); common ratios: 80/20, 65/35, 50/50, 35/65 |
| Weaving Method | Woven — plain weave, twill weave, satin weave, canvas construction |
| Common Yarn Count | T 21S/2, T 32S/2, C 21S/2, C 32S/2 (double-ply dominates for strength) |
| Common Density | Warp 80–120 ends/inch × Weft 60–90 picks/inch |
| Width | 140–220 cm (standard 150 cm) |
| Constructions | Plain (thin/dense), 2/1 twill (medium), 3/1 twill (thick/soft), canvas (heavyweight) |
Basic Specifications
| Parameter | Light (Shoe Lining / Garment) | Medium (Bags / Shoe Upper) | Heavy (Industrial / Work Shoes) |
| Basis Weight | 120–180 g/m² | 180–280 g/m² | 280–400+ g/m² |
| Thickness | 0.25–0.45 mm | 0.45–0.70 mm | 0.70–1.20 mm |
| Yarn Count | 32S/2 × 32S/2 | 21S/2 × 21S/2 | 16S/2 or coarse single |
| Blend Ratio | 65T/35C or 50/50 | 80T/20C or 65/35 | 100%T or 80T/20C |
| Construction | Plain weave | 2/1 twill | 3/1 twill / canvas |
Physical & Mechanical Properties
| Performance Indicator | Typical Value | Notes |
| Tensile Strength (Warp) | 600–1,200 N/5cm | Warp significantly higher than weft (woven nature) |
| Tensile Strength (Weft) | 400–800 N/5cm | Approx. 60–70% of warp |
| Tear Strength (Warp) | 30–80 N | Lower than nonwoven (limited yarn slippage) |
| Tear Strength (Weft) | 25–70 N | Same as above |
| Burst Strength | 800–2,000 kPa | Highest in canvas construction |
| Elongation | 15–35% (warp), 20–40% (weft) | Low elasticity, essentially non-stretch |
| Bending Stiffness | Medium–High (crisp hand) | Depends on cotton content and thickness |
| Dimensional Stability | Excellent (thermal shrinkage <1.5%) | Polyester component provides thermal-set stability |
| Abrasion (Martindale) | 20,000–80,000 cycles | Depends on density and blend ratio |
Comparison with Other Substrates
| Dimension | TC Woven | Needle-Punched | Spunlace | Warp-Knitted Pile |
| Structure | Warp × Weft interlaced | Fiber entangled | Hydroentangled | Knitted + raised pile |
| Directionality | Strong (warp/weft differ) | None (isotropic) | None | Yes (MD/TD) |
| Elasticity | Almost none | None | Low | Can be elastic |
| Hand Feel | Crisp, structured | Full, leather-like | Very soft, smooth | Fluffy, pile feel |
| Cost | Low–Medium (among the lowest) | Medium | Medium–High | Medium–High |
| Best Process | PVC calendering, flame lamination | Full impregnation, microsuede | Thin laminates, apparel | PU laminate, nubuck/suede |
| Breathability | ★☆☆☆☆ (dense) | ★★★★★ | ★★★★★ | ★★★★☆ |
| Peel Strength | ★★★ (adhesion-based) | ★★★★★ (fiber interlock) | ★★★★☆ | ★★★★☆ |
Inquiry